We produce sintered SiC tubes, reaction bonded SiC tubes and recrystallized SiC tubes. Our recrystallized SiC products have a high purity, while our reaction bonded and sintered silicon carbide tubes have a high mechanical strength. Our silicon carbide tubes possess good wearability,a low thermal expansion coefficient, extreme corrosion resistance, wear resistance, thermal shock resistance, high hardness and self-lubricating properties.
Silicon carbide Tube:
1,Professional manufacturer.
2,long working life of silicon carbide tube.
3,best after sale service.
Silicon Carbide Tube Applications
-Silicon carbide is frequently used in semiconductor and coating industries.
-SiC tubes are used to serve as components in industrial furnaces and thermal couple protectors.
-It can be used in high temperature applications.
Specifications about the silicon carbide pipe:
1. Best producing technology in China. Our tubes can be instead of Japanese tubes in Aluminium melt furnace.
2 Very smooth surface to avoid any blotted metal liquid.
3. Good thermal conductivity.
4. High tempreature strength.
5. Special groove to be easy fixed.
silicon carbide tube is mainly used in the production of aluminum, copper and zinc , as the lining material of the molten pool and electrolytic bath (reduction bath).The side lining of the reduction bath is eroding by aluminum and cryolite (used as additive), but Si3N4 bonded SiC material could not be eroded by aluminum, and do not have chemical reaction with cryolite.So this kind of material is ideal for the lining bricks of the electrolytic bath.In particular this kind of bricks have the excellent properties of high strength, abrasive resistance and nonconductive, so the copolymer (Al2O3 and Cryolite). The copolymer likes protective film to protect the working lining and improve the service life of electrolytic bath of silicon carbide pipe.At the same time, the Si3N4 bonded SiC bricks have lower thermal conductivity than silicon bricks, so they can reduce the thickness of the side wall or input higher power to expanse the loading capacity of the electrolytic bath, and to increase the output.Because of the high resistivity of the material, it can reduce the power consumption of the side -wall about 15%, saving energy and protecting environment on the silicon carbide tube.
Silicon Carbide Tube Specifications
Recrystallized SiC | Sintered SiC | Reaction Bonded SiC | |
Purity of Silicon Carbide | 99.5% | 98% | >88% |
Max. Working Temp. (`C) | 1650 | 1550 | 1300 |
Bulk Density (g/cm3) | 2.7 | 3.1 | >3 |
Appearance Porosity | <15%> | 2.5 | 0.1 |
Flexural strength (MPa) | 110 | 400 | 380 |
Compressive strength (MPa) | >300 | 2200 | 2100 |
Thermal expansion (10^-6/`C) | 4.6 (1200`C) | 4.0 (<500> | 4.4 (<500> |
Thermal conductivity (W/m.K) | 35~36 | 110 | 65 |
Main characteristics | High temp. High resistance. High purity | Fracture Toughness | Chemical Resistance |